EN AW 5754 (AlMg3) rolled aluminium plate
Rolled aluminium plates

EN AW 5754 (AlMg3) rolled aluminium plate

Easy to form, characterised by excellent corrosion resistance (also in outdoor and marine environments), with good formability and good weldability. Frequently used for simple cladding and covers.

  • Excellent corrosion resistance – especially in chloride/marine environments.
  • Good formability – reliable in both soft and half-hard tempers.
  • Good weldability – stable weld, low cracking tendency.
  • Can be anodised / painted – the colour shade may differ in decorative anodising.
Field of use
  • Food industry
  • Simple cladding
  • Decorative elements
  • Shipbuilding
Alloy grade
EN AW 5754 (AlMg3)
Tempers
H111 (soft), H22 (quarter-hard)
Thicknesses
Available sizes are listed on the product datasheets.
Formats
In plate and/or coil form.
Typically rolled execution, but also available as cast + milled.

EN AW-5754 – chemical composition1

(EN 573-3)

Specifications (%)

Remainder: Aluminium

Others
Si Fe Cu Mn Mg Cr Ni Zn Ti Ga V Notes Each Total2
0,40 0,40 0,10 0,50 2,60 - 3,60 0,30 - 0,20 0,15 - - 0,10 - 0,60 Mn+Cr 0,05 0,15
1 Chemical specifications are in mass %. Where no range is given, the alloying content is the maximum value.
2 Includes all elements for which no separate limit is specified.

EN AW-5754 – mechanical properties (H111 / H22)

DIN EN 485-2:2009-01
EN 485-2:2008

Temper Nominal thickness
t [mm]
Tensile strength
Rm min. [MPa]
Proof strength
Rp0,2 min. [MPa]
Elongation
A50 or A min. [%]
Bend factor 90°
rmin [·t]
Hardness
HBW
H111 0,2 – 0,5 190 80 12 0 · t 52
0,5 – 1,5 190 80 14 0,5 · t 52
1,5 – 3,0 190 80 16 1,0 · t 52
3,0 – 6,0 190 80 18 1,0 · t 52
6,0 – 12,5 190 80 18 2,0 · t 52
12,5 – 100,0 190 80 17 — 52
H22 0,2 – 0,5 220 130 7 1,5 · t 63
0,5 – 1,5 220 130 8 1,5 · t 63
1,5 – 3,0 220 130 9 2,0 · t 63
3,0 – 6,0 220 130 10 1,5 · t 63
6,0 – 12,5 220 130 11 2,0 · t 63
12,5 – 40,0 220 130 9 — 63

Notes:
• The table contains processed, condensed data from EN 485-2.
• Ahol A50 value is not given, the standard specifies the “A” (elongation) value.
• Bend radius values are indicative (rmin ≈ k·t).
• HBW: Brinell hardness with carbide ball.

EN AW-5754 – Al Mg3 – general alloy grade information

The values and data below are indicative – they help to give a general picture of the material.

Alloy designations

EN AWAl Mg3
Old designationAl Mg3
Material number (DIN)3.3535
United Kingdom (BS)-
Italy (UNI)-
SpainL-3390
Sweden144133
Norway-
France (AFNOR)A-G3M
Colour code RAL 1023   Traffic Yellow

Typical physical properties

Density [g/cm3]2,67
Modulus of elasticity [GPa]70,5
Thermal conductivity [W/m*K]140 – 160
Thermal expansion coefficient [K-1*10-6] -50°C – 20°C
20°C – 100°C   |   23,9
20°C – 200°C
20°C – 300°C
Specific heat [J/(kg*K)]-
Electrical conductivity [m/Ω*mm2]20 – 23
Shear modulus [GPa]26,5

Heat treatment

Annealing / recrystallisation annealing
Annealing temperature360°C – 380°C
Heat-up time1 – 2 hours
Cooling conditionsfurnace – not controlled
Hardening
Solution heat treatment-
Quenching-
Natural ageing-
Artificial ageing-
Machinability
Annealed3
Work-hardened2
Heat-treated-
Dimensional stability3
EDM1
Surface treatment
Anodising – protective1
Special anodising quality (EQ)1
Anodising – decorative2
Painting / coating3
Polishing1 – 2
Weldability
Process Value Filler metal
Gas2
TIG1SG-Al Mg3
MIG1SG-Al Mg5
Resistance welding3
Solderability
Brazing with flux4 – 5
Brazing without flux4
Abrasion soldering3
Soft soldering with flux4 – 5
Corrosion resistance
Normal atmosphere1
Marine environment1 – 2
Formability
Cold forming Value Delivery temper
Bending2
Compression forming3
Deep drawing2O
Upsetting2H12
Impact extrusion4
Hot forming
Closed-die forging3
Extrusion4
Hammer forging2
Food-contact use (DIN EN 602) yes

Legend

1very good
2good
3medium
4poor
5not suitable
EQ Anodising quality must be ordered separately and confirmed in writing

Thickness tolerances for rolled plates

EN 485-3:2003

Nominal thickness
t [mm]
Thickness tolerances by nominal plate width
[mm]
≤ 1 250 > 1 250 – 1 600 > 1 600 – 2 000 > 2 000 – 2 500 > 2 500 – 3 500
≥ 2,5 – 4 ± 0,28 ± 0,28 ± 0,32 ± 0,35 ± 0,40
4 – 5 ± 0,30 ± 0,30 ± 0,35 ± 0,40 ± 0,45
5 – 6 ± 0,32 ± 0,32 ± 0,40 ± 0,45 ± 0,50
6 – 8 ± 0,35 ± 0,40 ± 0,40 ± 0,50 ± 0,55
8 – 10 ± 0,45 ± 0,50 ± 0,50 ± 0,55 ± 0,60
10 – 15 ± 0,50 ± 0,60 ± 0,65 ± 0,65 ± 0,80
15 – 20 ± 0,60 ± 0,70 ± 0,75 ± 0,80 ± 0,90
20 – 30 ± 0,65 ± 0,75 ± 0,85 ± 0,90 ± 1,0
30 – 40 ± 0,75 ± 0,85 ± 1,0 ± 1,1 ± 1,2
40 – 50 ± 0,90 ± 1,0 ± 1,1 ± 1,2 ± 1,5
50 – 60 ± 1,1 ± 1,2 ± 1,4 ± 1,5 ± 1,7
60 – 80 ± 1,4 ± 1,5 ± 1,7 ± 1,9 ± 2,0
80 – 100 ± 1,7 ± 1,8 ± 1,9 ± 2,1 ± 2,2
100 – 150 ± 2,1 ± 2,2 ± 2,5 ± 2,6 —
150 – 220 ± 2,5 ± 2,6 ± 2,9 ± 3,0 —
220 – 350 ± 2,8 ± 2,9 ± 3,2 ± 3,3 —
350 – 400 ± 3,5 ± 3,7 ± 3,9 ± 4,2 —

Thickness tolerances for rolled plates

EN 485-3:2003

Nominal thickness
t [mm]
Thickness tolerances by nominal plate width
[mm]
≤ 1 250 > 1 250 – 1 600 > 1 600 – 2 000 > 2 000 – 2 500 > 2 500 – 3 500
≥ 2,5 – 4 ± 0,28 ± 0,28 ± 0,32 ± 0,35 ± 0,40
4 – 5 ± 0,30 ± 0,30 ± 0,35 ± 0,40 ± 0,45
5 – 6 ± 0,32 ± 0,32 ± 0,40 ± 0,45 ± 0,50
6 – 8 ± 0,35 ± 0,40 ± 0,40 ± 0,50 ± 0,55
8 – 10 ± 0,45 ± 0,50 ± 0,50 ± 0,55 ± 0,60
10 – 15 ± 0,50 ± 0,60 ± 0,65 ± 0,65 ± 0,80
15 – 20 ± 0,60 ± 0,70 ± 0,75 ± 0,80 ± 0,90
20 – 30 ± 0,65 ± 0,75 ± 0,85 ± 0,90 ± 1,0
30 – 40 ± 0,75 ± 0,85 ± 1,0 ± 1,1 ± 1,2
40 – 50 ± 0,90 ± 1,0 ± 1,1 ± 1,2 ± 1,5
50 – 60 ± 1,1 ± 1,2 ± 1,4 ± 1,5 ± 1,7
60 – 80 ± 1,4 ± 1,5 ± 1,7 ± 1,9 ± 2,0
80 – 100 ± 1,7 ± 1,8 ± 1,9 ± 2,1 ± 2,2
100 – 150 ± 2,1 ± 2,2 ± 2,5 ± 2,6 —
150 – 220 ± 2,5 ± 2,6 ± 2,9 ± 3,0 —
220 – 350 ± 2,8 ± 2,9 ± 3,2 ± 3,3 —
350 – 400 ± 3,5 ± 3,7 ± 3,9 ± 4,2 —
Note: We accept no liability or warranty for the correctness, accuracy or completeness of the information and data stated above. Standards and indicative values may change. Agreements are valid as set out in the quotation / order confirmation. We also draw attention to the fact that we accept no liability for colour shades arising during decorative anodising, or for corrosion-resistance results and how they develop. Individual terms may be agreed on a case-by-case basis and must be recorded in writing.